- Recycled thermoplastic elastomers
- 30% recycled content
- Black pellets
EcoTPE Strength is currently available in three variants, see table below:
Process guide:
- Drying is generally not necessary but can be carried out for approx. 3-4 hours at 70°
- Cylinder temperature: Injection molding is recommended at 180-210°
- Mold temperature: 30-60°C recommended temperature